Norsok L-002 Pdf
Remember:
A North Sea topside facility specified 316L stainless for a hot, high-chloride amine service. NORSOK L-002 Rev 4 clearly states (Clause 6.4.3) that 316L is not permitted for chlorides > 1000 ppm above 60°C. They were forced to retrofit with 6Mo CRA, costing $12 million. norsok l-002 pdf